Most rca's are like that. I just solder the return to the left edge of the barrel so that the return and signal conductors or the same length. Be careful not to get solder on the outside of the barrel as it may affect the fit of the collar.I use a hakko iron at 775F and for me I found it much harder to get a nice joint if I sink the barrel. If you use Q-dope it will keep the joint protected.