You can experiment with them...

The tape sticky shed syndrome is caused by the oxide coating peeling away or being delaminated from the tape. You could try to restore them by
baking them in the oven. According to some experts, you could set up the temperature in the oven at 130 F or thereabout to avoid melting the tape. Baking time should be around 6-8 hours again depending on the oven being used.



Edits: 12/23/20

This post is made possible by the generous support of people like you and our sponsors:
  Signature Sound   [ Signature Sound Lounge ]


Follow Ups Full Thread
Follow Ups

FAQ

Post a Message!

Forgot Password?
Moniker (Username):
Password (Optional):
  Remember my Moniker & Password  (What's this?)    Eat Me
E-Mail (Optional):
Subject:
Message:   (Posts are subject to Content Rules)
Optional Link URL:
Optional Link Title:
Optional Image URL:
Upload Image:
E-mail Replies:  Automagically notify you when someone responds.