In Reply to: RE: 40W Soldering Iron enough for Cardas CPBP Binding Posts posted by Palustris on March 8, 2021 at 10:38:59:
Agreed. I've been using the premium CCGR's for 10+ years now. At first they took forever to solder (I dial the temp up to 740/750 for these). What I learned to do is take a small abrasive Dremel bit (on a Dremel MINI MITE) to remove the plating from the cup. While the binding posts still take a good amount of time to heat up due to their mass, the overall soldering time is reduced applying solder to the exposed copper substrate.
This post is made possible by the generous support of people like you and our sponsors:
Follow Ups
- RE: 40W Soldering Iron enough for Cardas CPBP Binding Posts - alan m. kafton 12:13:53 03/08/21 (3)
- RE: 40W Soldering Iron enough for Cardas CPBP Binding Posts - pictureguy 12:40:48 03/08/21 (2)
- RE: 40W Soldering Iron enough for Cardas CPBP Binding Posts - alan m. kafton 14:45:13 03/08/21 (1)
- RE: 40W Soldering Iron enough for Cardas CPBP Binding Posts - pictureguy 15:19:37 03/08/21 (0)