Anybody have a simple/cheap way of removing the invisible enamel on Litz Wire? Would coating with Rosin Flux Paste prior to tinning help?
Follow Ups:
I just use a nice hot tip. Never really had a problem.
iBasso DX100,DX50 DX90. Chord Hugo. HiFiman 901 balanced. RSA Intruder, The Lightning. Fostex TH900 balanced, Hifiman HE-6, 560, JH13 Pro balanced. Lyr2, Audeze. All phones balanced. Whiplash cables.
Photo gallery: www.pbase.com/jamato8
I use paint stripper (don't have a solder pot), soaking the wire for a couple of hrs, moving it periodically. I've not been able to tell when it comes off cos its invisible, but it comes out looking sparkly new ie I cann't say what is an optimum soak time. You would v likely use a different paint stripper to me anyway.
It could be considered an unnecessary, but I clean the wire with methanol/lab grade before proceeding.
Lay the wire on an aspirin and hit it with the hot iron prepped with a blob of solder. Try not to inhale.
Asprin is an acid, and works well on soldering things to a steel chassis, but I wouldn't use it on copper without extensive cleaning afterwards.
I use a Weller soldering gun. I use a lot of litz wire. My wire has teflon cover so can take the high heat.
uses it in a well ventilated area.
Forgive my ignorance in asking this question. What happens to the insolation when you dip the wire in the pot? (I am considering buying one, but I have never used one.)
Dave
It simply melts right off and is replaced by the solder in the pot (tinning the wires!).
It's kind of a cheat to do it this way; the insulation in melted solder smells bad, but after 32+ years around a soldering iron/soldering pot, it is no worse than the smell of solder to this Dman's nose!
I'm sure that in the long run, this can't be good for my lungs...
Dman
Analog Junkie
Thanks! That does look like the way to go with Litz wire. I can imagine that someone would want to strip it strand by strand.
Dave
but in my experience it was inefficient at stripping the enamel and left a gooey mess that was even more difficult to deal with, on very thin gauge Litz type phono wires. I went back to sand paper followed by manual tinning. Possibly solder pot works better on thicker wires.
for phono cables (cardas), i melt.a blob of solder on 700degree tip. dip cable end w.insulation on into external flux amd stick into molten solder to tin wire.
nt
Dman
Analog Junkie
Get a solder pot, you will never have to strip a wire for tinning again.